Titanium 5-2.5

5Al-2.5Sn (Grade 6)

Material Data Sheet

Grade 6 Ti-5Al-2.5Sn alloy has high service temperature of 480°C (896°F), medium strength, and excellent weldability and fabricability. This alloy has good oxidation resistance and microstructure stability; however it is not heat-treatable.

Chemical Composition
Element Content (%)
Titanium, Ti 89.85 – 94
Aluminum, Al 4-6
Tin, Sn 2-3
Iron, Fe ≤ 0.50
Oxygen, O ≤ 0.20
Carbon, C ≤ 0.10
Nitrogen, N ≤ 0.030
Hydrogen, H ≤ 0.015
Other, each ≤ 0.050
Other, total ≤ 0.30
Physical Properties
Properties Metric Imperial
Density 4.48 g/cm3 0.162 lbs/in3
Melting Point ≤ 1590°C ≤ 2890°F
Mechanical Properties
Properties Metric Imperial
Tensile strength 517 MPa 75000 psi
Yield strength 827 MPa 120000 psi
Elastic modulus 110 – 125 GPa 16000 – 18100 ksi
Shear modulus 48 GPa 6960 ksi
Elongation at break 15% 15%
Hardness, Brinell 320 320
Hardness, Knoop 363 363
Hardness, Rockwell C 36 36
Hardness, Vickers 349 349
Thermal Properties
Properties Metric Imperial
Thermal expansion co-efficient (@0.000-100°C/32-212°F) 9.40 µm/m°C 5.22 µin/in°F
Thermal conductivity 7.80 W/mK 54.1 BTU in/hr.ft².°F
Applications

Grade 6 Ti-5Al-2.5Sn alloy is used in the following application areas:

  • Gas turbine engine casings and rings
  • Aerospace structural parts, aircraft engine and airframe.
  • Chemical processing equipment
Other Designations

Equivalent materials to grade 6 Ti-5Al-2.5Sn alloy are as follows:

  • ASTM B265 Grade6
  • ASTM B348 Grade6
  • ASTM B381 Grade6
  • MIL-T-9046
  • MIL-T-9047
  • AMS 4926
  • AMS 4910
  • AMS 4966
  • AMS 4953
  • MIL F-83142
  • MIL T-81556
  • MIL T-81915

Key Words: Ti 5-2.5, 5-2.5, 5Al 2.5 Sn, UNS R54520, Grade 6